Preparation Of Black Amorphous Silica From Rice Husks

The formation of black (carbon containing) amorphous silica from rice husks has been studied in detail. Three parameters: (i) purity, (ii) temperature of calcination and (iii) rate of heating have been found to affect the formation of black silica. The formation of black silica is higher in untreated rice husks than that in acid treated rice husks. The tendency to form black silica increases with the increase in the heating rate and the temperature of calcination of untreated rice husks. By treating with 3N HCl acid the formation of black silica can be avoided. Using a dopant/catalyst, black amorphous silica stable in air up to 1000 deg C was prepared from acid treated rice husks.

Author
R V Krishnaro Et Al
Origin
Defence Metallurgical Research Labs, Hyderabad, India
Journal Title
Trans Indian Ceram Soc 60 2 April-June 2001 95-99
Sector
General
Class
G 2563

Request article (free for British Glass members)

Preparation Of Black Amorphous Silica From Rice Husks
Trans Indian Ceram Soc 60 2 April-June 2001 95-99
G 2563
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
18 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.