Preparation And Optical Properties Of Transparent Glass-Ceramics Containing Cobalt (Ii) Ions

Transparent glass-ceramics containing ZnAl2O4:Co2+ and LiGa5O8:Co2+ crystallites have been prepared by heat treatment of glasses in the zinc aluminosilicate and lithium gallate silicate systems, respectively.