Preparation And Characterization Of Silica Aerogels/Glass Wool Composites

Using industrial water glass as silica source, silica aerogel/glass wool composite heat insulation materials were prepared through the gel moulding, surface modification and ambient pressure drying method. The microstructure and porous characteristics of the silica aerogel/glass wool composites were studied by scanning electron microscopy (SEM) and BET nitrogen adsorption-desorption method. The thermal conductivity of silica aerogel/glass wool composites was measured by the thermal conductivity measurement instrument. The results indicate that the as-prepared silica aerogel/glass wool composites exhibit strong hydrophobicity and excellent thermal insulation performance. The thermal conductivity of the obtained silica aerogel/glass wool composites is 1.1×10-2~2.0 W∙m-1∙K-1, and with the increasing of aerogels content, the thermal conductivity of the composites could be decreased further.

Author
H Zhang Et Al
Origin
Unknown
Journal Title
Advanced Materals Research 534 2012 106-109 www.Scientific.Net/Amr.534.106
Sector
Glass Fibre
Class
GF 702

Request article (free for British Glass members)

Preparation And Characterization Of Silica Aerogels/Glass Wool Composites
Advanced Materals Research 534 2012 106-109 www.Scientific.Net/Amr.534.106
GF 702
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.