Preparation Of Amorphus Silicas Doped With Organic Molecules By The Sol-Gel Prcess

Molecule disperation of amorphous siliceous materials doped with organic molecules were prepared by a sol-gel process in which (formula) was hydrolyzed in neutral or acidic solution.