Premix Technology For Improved Distribution Of Minor Materials

In this article, the author discusses premix technology and highlights its advantages and benefits. The company's experience in recent years has been that dosing and mixing accuracies of minor materials and their homogeneous distribution in the batch is particularly important to meet increased quality demands.

Author
Dr S Woltz
Origin
Eme, Germany
Journal Title
Glass International June 2018 28, 30-31