Premium Zircon - Reduction Of Internal Cracks

Reduction of internal cracks can be achieved by an alteration in particle size distribution of the batch material that is used to cast the ware.

Author
R Turner & C Daigler
Origin
Corning Refractories Plant
Journal Title
Glass Industry Development Int 2001 70
Sector
Refractories
Class
R 384

Request article (free for British Glass members)

Premium Zircon - Reduction Of Internal Cracks
Glass Industry Development Int 2001 70
R 384