Preliminary Thermoluminescence Investigation Of Commercial Pharmaceutical Glass Containers Towards The Sterilization Dosimetry Of Liquid Drugs

Drug sterilization with ionizing radiation is a well-established technology, which is constantly extending to several products due to its numerous advantages, since it allows the heat-free sterilization of heat-sensitive pharmaceutical preparations. In a previous study, the possibility to identify irradiated solid-state drugs by means of OSL and TL was examined with very promising findings. In the same respect, the present work aims, for the first time to the authors’ best knowledge, to explore whether TL can be employed as a method for post-sterilization dosimetry on commercial liquid-state drugs, by studying the properties of their glass containers. Two different types of glass containers (bottle and ampoule) of two widely used liquid drugs, i.e., Hexalen® and Voltaren®, are used for this purpose. Both glass containers exhibit a linear TL dose response for doses up to 6 kGy with a stable behavior through time, no significant sensitization of the main peaks is observed. Thus, preliminary findings are very promising towards the post-sterilization dosimetry of liquid drugs and the use of the containers of commercial liquid drugs for normal and/or accidental dosimetry.

Author
Un-named
Origin
Unknown
Journal Title
Applied Radiation & Isotopes www.Sciencedirect.com/Science/Article/Pii/S0969804315301457
Sector
Container glass
Class
C 5526

Request article (free for British Glass members)

Preliminary Thermoluminescence Investigation Of Commercial Pharmaceutical Glass Containers Towards The Sterilization Dosimetry Of Liquid Drugs
Applied Radiation & Isotopes www.Sciencedirect.com/Science/Article/Pii/S0969804315301457
C 5526
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.