Predictive Modelling Of Liquids Spreading On Solid Surfaces

A liquid spreading model is developed in which surface and gravitational driving energies are balanced against the energy lost through bulk viscous dissipation. Behaviour is described in terms only of independently measurable quantities, with no adjustable parameters. Additionally, the model can be used to predict liquid viscosity as a function of spreading behaviour.

Author
M Denesuk Et Al
Origin
Donnelly Corp, Usa
Journal Title
Physics And Chemistry Of Glasses 34 5 1993 203-241
Sector
Special Glass
Class
S 768