Precision Manufacture For Flat Screen Developments

The manufacture of high precision flat glass for such products as flat panel displays and digital optical discs is described with reference to the procedures employed by Pilkington Micronics Ltd of Deeside.

Author
W Marsden
Origin
Unknown
Journal Title
Glass July 1990 245-247
Sector
Flat glass
Class
F 230

Request article (free for British Glass members)