Practicle Guide For The Assessment Of Glass Making Sands: Part 1 - Procedures For Sampling And Physical Testing

A practicle guide for glass makers for the assessment of sands intended for both those with their own laboratory facilities and those sampling sand for subsequent assessment by an outsourced laboratory. Guidance is offered for a variety of glass-making activities with the intention of providing a basis for the assessment of both the continued supply of established sands and the evaluation of new sources of silica sand. Part 1 addresses sampling and physical testing; including the determination of moisture, inspection for contamination and particle size analysis.

Author
M West
Origin
West X-Ray Solutions, Sheffield
Journal Title
Glass Technology: European Journal Of Glass Science And Technology Part A, Vol 51, No 2, April 2010
Sector
Special Glass
Class
S 3895

Request article (free for British Glass members)

Practicle Guide For The Assessment Of Glass Making Sands: Part 1 - Procedures For Sampling And Physical Testing
Glass Technology: European Journal Of Glass Science And Technology Part A, Vol 51, No 2, April 2010
S 3895
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.