Practical Strength Of Glass Containers. Part 2 - Influence Of Handling

The practical strength of container glass depends not only on the stress distribution at the surface, but also on the type and distribution of surface defects. After the elimination of the influence of the container shape by means of finite element methods, different types of defect show a different behaviour in the Weibull plot. This behaviour can be used to compare different handling materials.

Author
J Wagner Et Al
Origin
Fachbereich Werkstofftechnik, Germany
Journal Title
Glastech Ber Glass Sci Technol 67 7 1994 197-201
Sector
Container glass
Class
C 687

Request article (free for British Glass members)

Practical Strength Of Glass Containers. Part 2 - Influence Of Handling
Glastech Ber Glass Sci Technol 67 7 1994 197-201
C 687
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.