Pr3+/Er3+ Codoped Ge-As-Ga-S Glasses As Dual-Wavelength Fibre-Optic Amplifiers For 1.31 And 1.55 Um Windows

Fluorescence emissions at both 1.31 and 1.55 um communication windows were observed from Pr3+/Er3+ codoped Ge-As-Ga-S glasses with a single wavelength pumping at 986nm.

Author
S H Park Et Al
Origin
Pohang University, Republic Of Korea
Journal Title
J Am Ceram Soc 83 5 2000 1284-1286