PPG Industries recently announced that it has developed a glass with self-cleaning properties called SunClean glass for residential window applications. The new glass provides two consumer-valued benefits: windows with SunClean are easier to clean and stay cleaner so homeowners have less hassle. The self-cleaning properties are made possible by a durable, transparent coating of titanium dioxide applied during the manufacturing process.