The Power To Deliver

It is of paramount importance that a glass conditioning unit, whether forehearth or working end, is able to deliver the required heating and cooling. It is likewise imperative that those requirements correctly anticipate all likely heating and cooling scenarios. This article describes how these aims are achieved.