Powdering System For Curved Mirrors

Germany's IfG Ingenieurbuero fur Glastechnik GmbH recently supplied two additional vertical systems for a line in Pittsburgh, USA, used to manufacture curved solar mirrors for solar power plants. The vertical EPS powdering system provides precision application of interleaving powder precisely. Other claimed benefits are the perfect adhesion of powder to the mirrors and low operational costs. According to the firm, these process parameters determine the quality, performance and durability of solar mirrors.

Author
Un-named
Origin
Unknown
Journal Title
Glass Worldwide May-June 2010 6
Sector
News Items
Class
N 2472