Postmortem Analysis Of Magnesia And Magnesia Zircon Checker

In this article the authors discuss the postmortem analysis of magnesia and magnesia zircon checkers after one campaign in a soda-lime glass melting furnace.

Author
R Bei Et Al
Origin
Rhi Glas, Germany
Journal Title
Glass Worldwide July-August 2015 72, 74, 76
Sector
Refractories
Class
R 839