A Possible New Interpretation Of The Structure Of Borate Glasses

The original model of the sodium borate glass structure, proposed by the authors some years ago, is briefly summarised and some of its advantages underlined. Evidence is presented for the existence of two roles for sodium oxide with opposing effects upon the structure and properties. The variation of basicity with the composition of sodium borate glasses was examined. Basicity data from different sources, including those of the present authors, are presented.

Author
P Balta & D Radu
Origin
University Politehnica Of Bucharest
Journal Title
Phys Chem Glasses 41 5 2000 278-281
Sector
Special Glass
Class
S 2059

Request article (free for British Glass members)

A Possible New Interpretation Of The Structure Of Borate Glasses
Phys Chem Glasses 41 5 2000 278-281
S 2059
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.