Possibility Of Using Calcium Metasilicate From A Phosphorus Furnace For The Production Of Containers In Amber Glass (Part 2) (Italian)

The importance of sulphur-containing additives for colour stability and optical properties, particularly dominant wavelength and ultraviolet transmission, is discussed.