Possibilities Of Determining Sio2 And Na2O By Means Of X-Ray Fluorescence Analysis.

The possibilities of using XRF for the determination of SiO2 and Na2) in glasses of the system Si2-B2O3-Na2O have been explored. Tests have shown that in spite of the apparently simple system, results are not yet as accurate as desired but the speed of XRF determination compared with other methods justifies its use.