Porous Aluminia-Based Ceramic

The possibility of producing strong porous ceramics based on aluminium oxide is shown. SiC with an activating additive and ammonium bicarbonate are used as a binder and a pore agent, respectively. The effect of the amount of the additives thus introduced and firing temperature on the porosity and strength of the material is studied.

Author
E M Tomilina Etal
Origin
Mendeleev Russian Chemical Engineering University, Moscow, Russia
Journal Title
Glass And Ceramics 57 5-6 2000 210 - 212
Sector
Glass Ceramics
Class
GC 677

Request article (free for British Glass members)

Porous Aluminia-Based Ceramic
Glass And Ceramics 57 5-6 2000 210 - 212
GC 677