Polysulphide In Large-Scale Ig Glazing

Architects are designing new buildings with more glazing in their facades. In particular, the use of insulating glass is widespread because of its potential for saving energy. According to the authors, the success of insulating glass is closely linked to the development of the liquid polymer polysulphide Thiokol, the most widely used raw material for edge sealants.

Author
H Lucke & R Schmidt
Origin
Morton International , Germany
Journal Title
Glass-Tech Int 2/97 143-145
Sector
Flat glass
Class
F 722