Polyphosphates Glasses In Enameling Process Of Melts

Polyphosphates glasses have good resistance properties in liquid metal bath. This property makes them attractive as steel protection agents against corrosion in such media. The aim of this work is to develop a new coating process of steel, starting from polyphosphates coacervates.