Polish Refractories - The Switch To Imports - Refractory Raw Materials Consumption In Poland

This paper focuses on significant changes in raw materials usage in the Polish refractory industry in the last 10-15 years.

Author
K Galos
Origin
Polish Academy Of Sciences
Journal Title
Industrial Minerals 397 October 2000 57, 59-65
Sector
Refractories
Class
R 372