Plm'S Success With Indirect Batch And Cullet Preheating

In a joint project with the German state, PLM has installed a sophisticated waste heat utilisation system at its Munder glassworks. The principal part of the system is an indirect Zippe cullet preheater, which, depending on the ratio of cullet melted, has provided energy savings of up to 18%.