Platinum Feeders In The Danner Process

To improve the quality of tubing it is essential that manufacturing tolerances are extremely tight. Eglass Platinum Technology suggests the use of a platinum feeder based on the DHPS concept in place of a conventional ceramic feeder.

Author
E Schotz
Origin
Eglass Platinum Technology Gmbh, Germany
Journal Title
Gmpa 4/98 189-192
Sector
Container glass
Class
C 1219