[Plastics] Palandri Cheer Pack

Palandri is responsible for the latest development in wine packaging, the Cheer Pack. This fully recyclable container is made from plastic and aluminium foil, and can be made in any size between 187ml to 1 litre. The Cheer Pack is the result of 18 months research and will first be exported to Canada, but there are plans to make use of this packaging elsewhere. In addition to being recyclable, the Cheer Pack is resealable. It can also be flattened to reduce landfill space, an issue of particular concern to the Canadian government.

Author
Un-named
Origin
Unknown
Journal Title
The Drinks Business Jan/07 72
Sector
Packaging Abstracts
Class
PA 107