Plans For The Automation Of Annealing Lehrs In The Glass Industry

A Discussion of the literature leads to the conclusion that the main requirement for good annealing is good temperature control in the lehr, assuming controlled gas pressure. The article is a plea for more control on lehrs in East Germany.

Author
W Liehn
Origin
Unknown
Journal Title
Silikattechnik 10 6 1959 280