Pill Poppers - Pharmaceutical Packaging Demand Analysis

This article looks at how China, India and Indonesia's leading glass manufacturers are emerging as specialists in pharmaceutical glass packaging. The three regions are drawing the world's major multinational pharma glass makers and the movement looks set to continue, given a host of favourable trends in the region, as explained here.

Author
Un-named
Origin
Unknown
Journal Title
Asian Glass Dec-Jan 2015 30-32, 34-35