Pilkington Planar

The glass giant has declared that Planar Triple is the most impressive yet in the range. It is claimed to be the first triple glazed frameless structural glazing system. With an acoustic performance of Rw>42dbA and achievable "U" values of 0.8W/m2K, the system allows the incorporation of a wide range of glass types and support systems, such as glass mullions, aluminium and steel purlins and rigging, without compromising either the aesthetic appeal or thermal performance.