Physicochemical Properties And Structue Of Ga2S3-Ge22-La2S3 Glasses (Ln=Ytrrium Or Lanthanoids)

Physicochemcial properties - crystallisation and glass transition temperatures, molar volume, molar refraction and Vichers hardness - were studied for Ga2S3-GeS2-La2S3-LnS3 glasses.