Physical Properties Of Chalcogenide And Chalcohalide Glasses

The physical properties of glasses in the Ge30As10Se(60-x)Tex system with x=25, 28, 30, and 35 at.% Te, the Ge30As10Se30Te(30-y)Iy system with y=5, 10, 20, and 30 at.%I, the Ge30As10Se35Te(25-z)Iz system with z=2, 6, 10, and 20 at.% and the [Ge30As10Se30Te30]Iw system with w=0, 5, 10 and 20at.% I have been investigated. The changes in the glass transition temperature, density, coefficient of thermal expansion, hardness, and viscosity are attributed to the delocalized metallic bonding character of Te in the subsitution of Te for Se in the Ge-As-Se-Te glass system and the network-terminating role of iodine in the substitution of I for Te in the Ge-As-Se-Te-I glass system, respectively.

Author
V Q Nguyen Et Al
Origin
Virginia Polytechnic Inst, Usa
Journal Title
J Am Ceram Soc 83 4 855-859
Sector
Special Glass
Class
S 1902

Request article (free for British Glass members)

Physical Properties Of Chalcogenide And Chalcohalide Glasses
J Am Ceram Soc 83 4 855-859
S 1902
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.