Physical Properties Of Barrier Ribs Of Plasma Display Panels: Ii, Effects Of Fillers

The effects of inert fillers, such as quartz and Al203, on the sintering behaviour and physical properties of lead borosilicate glasses used for barrier ribs of plasma display panels (PDP) were investigated. The effects of volume fraction and type of filler on the sintering temperature, thermal expansion coefficient, dielectric constant and fracture resistance of the barrier ribs of PDP were investigated. The influence of the filler on sintering behaviour was discussed based on the wetting angle of glass onto the fillers. The physical properties and fracture resistance of the glass with fillers were measured and compared with theoretical models.

Author
G Hwang Et Al
Origin
Hongik University, Seoul
Journal Title
J Am Ceram Soc 85 12 2002 2961-2964
Sector
Special Glass
Class
S 2472

Request article (free for British Glass members)

Physical Properties Of Barrier Ribs Of Plasma Display Panels: Ii, Effects Of Fillers
J Am Ceram Soc 85 12 2002 2961-2964
S 2472
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.