Physical Meaning Of The So-Called Kinetic Compensation Effect

It is shown that the kinetic compensation effect (for conductivity called Meyer-Nelder thermodynamic compensation rule) mathematically results from the exponential form of the Arrhenius rate constant and certain types of approximations. A change of activation energy is thus compensated by the same change in the logarithm of the pre-factor. As an example, resulting temperature dependence of field effect and the activation energy can service to demonstrate a useful tool for the estimation of the role of the interface states while investigating insulator (Si02 or SiNx) and amorphous (glassy) semiconductor (a-Si).

Author
J Sestak Et Al
Origin
Czech Acad Sciences, Prague
Journal Title
Glastech Ber Glass Sci Technol 73 C1 2000 104-110
Sector
Special Glass
Class
S 2488

Request article (free for British Glass members)

Physical Meaning Of The So-Called Kinetic Compensation Effect
Glastech Ber Glass Sci Technol 73 C1 2000 104-110
S 2488
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.