Physical Chemistry Of Glass Surfaces

Considerable progress has been made in understanding the nature and behaviour of glass surfaces since the Xth ICG in Kyoto, Japan 1974. The excellent Rolla Conference or Glass Surfaces and proceedings therefrom, firmly established that the surface-environment interactions of glass can now be treated as a science. Characterization of the composition and structure of a glass surface has been made possible through the development of a number of new surface analysis techniques. Through the use of these tools it is now a firmly established fact that glass surfaces consist of complex compositional profiles of all the constituents in the glass. Bulk composition, melt history, fabrication variables such as furnace and lehr atmospheres, and environmental history all influence the compositional profiles characteristic of a given glass article. Direct relationships between surface compositional profiles and physical and chemical properties thus can be established. In fact, it is the ability to characterize the glass surface sufficiently to relate the surface to glass processing on the one hand and glass properties on the other that makes the study of glass surfaces a bona fide materials science.

Author
L L Hench
Origin
University Of Florida, Usa
Journal Title
J Non-Cryst Solids 25 1-3 1977 343-369
Sector
Primary Papers
Class
PP 1559

Request article (free for British Glass members)

Physical Chemistry Of Glass Surfaces
J Non-Cryst Solids 25 1-3 1977 343-369
PP 1559
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.