Physical & Chemical Properties Of Mesi03/2-Si02 Films Prepared By The Sol-Gel Method

Silica gel coating films containing various amounts of methyl groups were prepared using methyltriethoxysilane, MeSi(OEt)3, and tetraethoxysilane, Si(OEt)4, as starting materials. Incorporation of methyl groups into Si02 structure lowered the refractive index of the films. The refractive index of the films containing methyl groups decreased by 0.01-0.02 with heat-treatment at temperatures from 200-400 deg C and increased by about 0.02 at temperatures from 500-600 deg C.

Author
A Matsuda Et Al
Origin
Osaka Prefecture Univeristy, Japan
Journal Title
Proc Xviii Icg, San Francisco, Usa, July 1998 201-206
Sector
Special Glass
Class
S 1862

Request article (free for British Glass members)

Physical & Chemical Properties Of Mesi03/2-Si02 Films Prepared By The Sol-Gel Method
Proc Xviii Icg, San Francisco, Usa, July 1998 201-206
S 1862
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 14 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.