Phase Transitions And Transient Liquid-Phase Sintering In Calcium-Substituted Lanthanum Chromite

This paper investigates sintering and phase transitions of La0.7CaxCr03 (0.25

Author
L A Chick Et Al
Origin
Pacific Northwest Lab, Usa
Journal Title
J Am Ceram Soc 80 8 1997 2109-2120