Phase Separation, Crystallization, And Microwave Dielectric Properties Of Mgo-Al2O3-Sio2-Tio2-La203 Glass-Ceramic

The effects of heat treatment on phase separation, crystallisation, and microwave dielectric properties of the 1MgO.1.2Al2O3.2.8SiO2.1.4TiO2.O.2La2O3 (in molar ratio) glass and glass-ceramic were investigated. The results show that the parent glass has a two-liquid phase separation structure, with a droplet phase rich in Al & Ti embedded in the matrix rich in Si. Heat treatment of the glass at 770 deg C leads to the enlargement of the liquid droplets and promotes the formation of crystals from the droplets. The initial crystalline phase perrierite appears after heat treatment of the parent glass at 850 deg C, and it is analysed to precipitate from the Al&Ti-rich droplet phase. With increasing heat-treatment temperature from 850 deg C, to 1250 deg C, the crystallization degree of the glass increases as the other main crystal phases rutile, cordierite and magnesium aluminotitanate precipitate successively from the material.

Author
H Wang Et Al
Origin
Shanghai Inst Ceramics, China
Journal Title
Int J Appl Glass Sci 7 3 Sept/2016 328-336
Sector
Glass Ceramics
Class
GC 883

Request article (free for British Glass members)

Phase Separation, Crystallization, And Microwave Dielectric Properties Of Mgo-Al2O3-Sio2-Tio2-La203 Glass-Ceramic
Int J Appl Glass Sci 7 3 Sept/2016 328-336
GC 883
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 9 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.