Phase Separation And Structural Differences Between Alkali Silicate Glasses Parepared By The Sol-Gel And Melt-Quench Method

Glasses of the composition xM20:(1-x)Si02[M=Na,Li] with x=0.15 and 0.2 have been prepared both by the melt-quench and the sol-gel methods. X-ray photoelectron spectroscopy shows that with increasing sintering temperature the structure of gels approaches that of the melt-quench glass but does not become identical even on heating above the glass transition temperature (Tg).

Author
B Roy Et Al
Origin
Lehigh University, Bethlehem, Usa
Journal Title
J Am Ceram Soc 81 9 1998 2360-2370
Sector
Special Glass
Class
S 1537

Request article (free for British Glass members)

Phase Separation And Structural Differences Between Alkali Silicate Glasses Parepared By The Sol-Gel And Melt-Quench Method
J Am Ceram Soc 81 9 1998 2360-2370
S 1537
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.