This paper discusses recent developments in compositions and innovations in container manufacture which ensure that glass continues to be the material of choice. Type I sodium borosilicate glass is highly corrosion-resistant, and compositions with cerium oxide do not darken on exposure to gamma radiation used for sterilization. Press-and-blow forming enables containers to be made lighter and permits new designs which allow delivery of small doses of valuable products with minimum waste. Sophisticated on-line inspection equipment includes image recognition systems to control positively the quality of all bottles, one at a time. Statistical process control and adherence to ISO 9000 standards lead to further improvements in quality.

Author
J Wenzel
Origin
Rutgers University, Usa
Journal Title
Proc Xvii Int Cong Glass Beijing, Vol 6, October 1995 364-368
Sector
Container glass
Class
C 1125

Request article (free for British Glass members)

Pharmaceutical Glass Packaging
Proc Xvii Int Cong Glass Beijing, Vol 6, October 1995 364-368
C 1125
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.