Pet Packaging Market Report Published: New Research From Pira

A report by PIRA on global trends in PET packaging until 2007 consulted 97 leading polymer suppliers, bottle and sheet converters and end users in Europe. Beer is a growth market, driven extensively by China which by 2004 is expected to have overtaken the USA as the world's leading beer producer. Technological advance over five years will be critical t the development of new beer applications, and the use of small bottles for fresh juices, wine, flavoured alcoholic beverages and health oriented drinks will significantly increase. The EU market is expected to grow from its current 2.165 m/t to 3.297 m/t in 2007. More than 66% of the additional tonnage forecast will be where pet replaces other packaging materials. PET for food packaging is also considered to be a likely growth area.

Author
Un-named
Origin
Unknown
Journal Title
Active Intell Pack News 13 4 April 2003 7 (Pira Abstract July/03)
Sector
Container glass
Class
C 2249

Request article (free for British Glass members)

Pet Packaging Market Report Published: New Research From Pira
Active Intell Pack News 13 4 April 2003 7 (Pira Abstract July/03)
C 2249
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.