Pelletizing And Recycling Of Dust From And To A Lead Glass Furnace

OI-NEG TV Products is a leading manufacturer of glass funnels for the television picture tube envelope. The company produces over 10m units per year operating 365 days per year. This paper examines the pelletizing and recycling of dust from this company's furnaces, the dust collection rate averaging 3500 lb/day.