Particle Analyser Tests Raw Material Quality

The Elzone analyser is useful in a variety of applications within the glass industry. It has been used to test incoming raw materials to ensure their quality before milling as well as for the final milled product. Unlike laser particle size analysers, the Elzone analyser uses an electrozone sensing technique in which particles suspended in a conductive fluid flow one at a time through an orifice under a pressure differential. Electrodes are immersed on each side of the orifice and as each particle passes through, it displaces its own volume of electrolyte. This produces a detectable pulse in the electrical conductance across the orifice. The amplitude of the pulse is proportional to the volume of the electrolyte displaced by the particle and this is the actual volume of the particle. For more information contact Micromeritics (USA) fax: +770 662 3696.

Author
Un-named
Origin
Unknown
Journal Title
Glass 76 6 1999 187
Sector
News Items
Class
N 619

Request article (free for British Glass members)

Particle Analyser Tests Raw Material Quality
Glass 76 6 1999 187
N 619
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.