Packaging Of Beverages (In Italian)

The shelf life of beverages is governed by the rate of deterioration attributable to 3 main factors - microbial growth, interaction between the beverage and the outside environment, and interaction between the beverage's components and the packaging material. The major physicochemical and microbiological characteristics of mineral waters, fruit juices, carbonated drinks, cold tea, beer, energy drinks, wine and spirits are surveyed from the viewpoint of their packaging requirements, and suitable container materials are discussed. Particular reference is made to the use of PET.

Author
A Rossi
Origin
Unknown
Journal Title
Imballaggio No 521 22 May 2000 28-31
Sector
Container glass
Class
C 4531

Request article (free for British Glass members)

Packaging Of Beverages (In Italian)
Imballaggio No 521 22 May 2000 28-31
C 4531
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.