Oxygen Permeability Of Plastic Bottles For Oxygen Sensitive Beverages

Oxygen is one factor which causes beverages to deteriorate after filling. In particular, the replacement of glass bottles by plastic bottles has implications for the shelf life. As a consequence, packaging manufacturers and food technologists must have precise knowledge about the composition of packaging materials, oxygen permeation and the interaction between oxygen, the packaging and the foodstuffs. This article discusses the theory of permeation and factors influencing permeation. Results of oxygen permeation through plastic bottles and closures are presented. The results show that the 3 main methods for barrier improvement are internal coating of PET bottles, the use of PEN bottles and the incorporation of oxygen scavengers into bottles and closures. Finally, numerical simulations indicate that although oxygen scavengers are useful for reducing the oxygen ingress, their potential for reducing dissolved oxygen and preexisting oxygen in the headspace is limited.

Author
K Muller
Origin
Unknown
Journal Title
Monatsschr Brauwiss 60 506 2007 74-83
Sector
Container glass
Class
C 4505

Request article (free for British Glass members)

Oxygen Permeability Of Plastic Bottles For Oxygen Sensitive Beverages
Monatsschr Brauwiss 60 506 2007 74-83
C 4505
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.