Oxygen-Hydrogen Burners Improve Glass Surfaces

This study indicates their use in surface polishing treatments reduces roughness and improves container appearance.

Author
A Masella & F Virey
Origin
Unknown
Journal Title
Glass Industry April 1988 24-25
Sector
Primary Papers
Class
PP 1150

Request article (free for British Glass members)

Oxygen-Hydrogen Burners Improve Glass Surfaces
Glass Industry April 1988 24-25
PP 1150
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.