Oxygen Firing At Parkersburg

Experience in the use of oxygen firing on a 110 tpd tank melting a high-alkali borosilicate glass for glass fibre marbles is reported.

Author
D Shamp, D Davies
Origin
Manville Sales Corp
Journal Title
American Glass Review December 1990 6-9, 13
Sector
General
Class
G 526