Oxygen Bubble Development On A Platinum Electrode In Borosilicate Glass Melt By The Effect Of Alternating Current

A high-temperature observation of bubble evolution by the effect of mains alternating current (50 Hz) in borosilicate glass melt at temperatures of 1100 and 1225 deg C was completed by measurement of the polarisation curves and measurement of the mean electrode potential and potential course at electrodes fed by rectangular alternating current. The development of oxygen bubbles already starts at a current density of about 30 mA.cm-2. Above 100 mA.cm-2, fluctuations in bubble development occur and bubbles start to release from the electrode. Above 220-250 mA.cm-2, massive bubble evolution starts. Bubble development at 1100 deg C is considerably higher than at 1225 deg C and limits in their evolution are more noticeable. The limits in bubble development correspond to changes of potential course and of mean electrode potential. An explanation of the changes in electrode behaviour, based on an alternating transition between two mechanisms of oxygen development and/or on alternating reduction and re-forming of oxidic layer on the electrode in the transition range, has been suggested. Start of bubble evolution at low alternating current density has also been observed in simple sodium-calcium-silicate glass melt. A relation between bubble release and platinum corrosion caused by reduced silicon has been suggested.

Author
J Matej & M Jebava
Origin
Inst Chem Technology, Prague, Czech Republic
Journal Title
Ceramics Silikaty 58 4 2014 249-259
Sector
Special Glass
Class
S 4202

Request article (free for British Glass members)

Oxygen Bubble Development On A Platinum Electrode In Borosilicate Glass Melt By The Effect Of Alternating Current
Ceramics Silikaty 58 4 2014 249-259
S 4202
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
12 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.