Oxy-Gas Forehearths: Results Of Mathematical Modeling Of A Fling Glass And Field Trials On A Borosilicate Glass

This paper describes the results of mathematical modeling, burner development, & field trials carried out with oxy-gas forehearths. Mathematical modeling was carried out for the rear cooling section of a BH-F forehearth conditioning a flint glass. The modeling coupled the glass channel with the forehearth combustion space. The glass exit temperatures from this section were compared under air-gas firing & oxy-gas firing. Results indicated that for the same glass flow rates, cooling was more efficient in the centre of the channel & heating more efficient close to the sides under oxy-gas firing. The combined effect was a 30% improvement over air-gas firing in temperature spread at the exit of the cooling zone. Conversely, the model also predicted that for similar temperature spreads, oxy-gas firing would allow pull through to be increased by 30%

Author
A Stephens Et Al
Origin
Bh-F Engineering, Uk
Journal Title
Ceram Eng Sci Proc 20 1 1999 143-154
Sector
General
Class
G 3636

Request article (free for British Glass members)

Oxy-Gas Forehearths: Results Of Mathematical Modeling Of A Fling Glass And Field Trials On A Borosilicate Glass
Ceram Eng Sci Proc 20 1 1999 143-154
G 3636
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.