Oxy-Fuel Technology Applied To Art Glass

AGA AB and the Swedish glassmaker Orrefors Kosta Boda AB have worked together to introduce all oxy-fuel melting technology to art glass production. Test results from the first installation at a Boda furnace show a 55% reduction in oil consumption and an increase in melting rate and percent pack rate.