Oxide Ceramic Sintering Particulars

The sintering of intermediate powder articles based on oxide ceramic is examined from the standpoint of diffusion mass transfer. Two types of powders, differing by the preparation methods, are used in practice. As a rule, the more coarse powder is usually obtained by mechanical comminution while the other powder, characterised by a high dispersity and content of different types of crystal lattice defects in the particles, is obtained by chemical methods, such as precipitation from solutions, heterophase interaction, cryo- and plasma-chemical treatment, and so forth. It is shown that when intermediate articles are sintered they are compacted and hardened by different physical mechanisms.

Author
V S Bakunov & E S Lukin
Origin
Russian Academy Of Sciences, Moscow
Journal Title
Glass & Ceramics 68 7-8 Nov/2011 211-215
Sector
Glass Ceramics
Class
GC 771

Request article (free for British Glass members)

Oxide Ceramic Sintering Particulars
Glass & Ceramics 68 7-8 Nov/2011 211-215
GC 771
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
11 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.